Sdf Posted August 27, 2020 Report Share Posted August 27, 2020 If you know about this chemical please tell me...I hope with you all. Link to comment Share on other sites More sharing options...
Dick White Posted August 27, 2020 Report Share Posted August 27, 2020 If the glaze has been fired, it is permanent. No household or hardware store chemicals will remove it. If the glaze is just a mistake on the bisque ceramic, usually it will wash off with water. Link to comment Share on other sites More sharing options...