TonyC Posted October 15, 2019 Report Share Posted October 15, 2019 I am about to embark on some handbuilding exercises after completing a recent workshop. One of the styles requires a white slip atop a clay of choice. I would take any advice for the best clays for handbuilding, and then also the best white slip recipe for it to match. I have some Laguna WC608 clay at the house which I will use to start. I know that matching 'shrinkage' for clay and slip is an important characteristic and the WC608 has a 10.9% percentage (http://www.lagunaclay.com/clays/northeastern/wc608.php). Can anyone offer advice or other suggestions for these combinations? Thanks in advance. Link to comment Share on other sites More sharing options...