Aditi Posted February 19, 2019 Report Share Posted February 19, 2019 Can i let it sit for 4-5 days or does it have to be fired as soon as the glaze dries? Link to comment Share on other sites More sharing options...
Chilly Posted February 19, 2019 Report Share Posted February 19, 2019 Providing they are, and stay dry, you can leave it forever. Link to comment Share on other sites More sharing options...
Aditi Posted February 19, 2019 Author Report Share Posted February 19, 2019 Thank you! Link to comment Share on other sites More sharing options...
hitchmss Posted February 19, 2019 Report Share Posted February 19, 2019 If they sit in a dusty area for a long time, you might want to lightly blow them off with compressed air before loading into the kiln. Just a little air, not too much pressure! Link to comment Share on other sites More sharing options...