Adhithan Posted February 4, 2019 Report Share Posted February 4, 2019 Glaze pinhole in sanitary ware product only in some patterns,same glaze good for other all pattern tell me some remides to find out the problem Link to comment Share on other sites More sharing options...
neilestrick Posted February 4, 2019 Report Share Posted February 4, 2019 Can you put up a picture? Pinholes can vary a lot, and it would be good to make sure we're talking about the same thing. Also, where are you located, what type of kiln and atmosphere, and what cone? Welcome to the forum! Link to comment Share on other sites More sharing options...