PamelaLBL Posted March 14, 2018 Report Share Posted March 14, 2018 Has anybody used underglazes under a clear crackle Raku? Link to comment Share on other sites More sharing options...
Magnolia Mud Research Posted March 14, 2018 Report Share Posted March 14, 2018 Yes. It works just fine for decorative effects. Link to comment Share on other sites More sharing options...
PamelaLBL Posted March 15, 2018 Author Report Share Posted March 15, 2018 Thank you! Just glazed a few pieces to test next week. Link to comment Share on other sites More sharing options...
Axel Posted June 2, 2018 Report Share Posted June 2, 2018 On 3/14/2018 at 9:20 PM, PamelaLBL said: Thank you! Just glazed a few pieces to test next week. How did the underglazes come out under your clear raku glaze? Did you modify anything before application? Link to comment Share on other sites More sharing options...