carr pottery Posted June 7, 2017 Report Share Posted June 7, 2017 Looking for zinc free clear glaze for Standard 266. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 7, 2017 Report Share Posted June 7, 2017 here is one I used in Oxidation or reduction. Can't say whether it will work with Standard 266. It worked with ^6 porcelain and stoneware. semi gloss Clear ^6 Neph Syen 26.1 Gerstley Bor. 4.7 EPKaolin 19 Whiting 18.7 Silica 31.5 100 Marcia Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 7, 2017 Report Share Posted June 7, 2017 Here is Wayne Bates Clear ^6 Oxidation glaze SATIN MATT CLEAR R-1002 (^6 OX) Gerstley Borate 9 Strontium Carb 14 Wollastonite 14 Nepheline Syenite 35 EPK 9 Flint 19 total 100 Marcia Link to comment Share on other sites More sharing options...
carr pottery Posted June 7, 2017 Author Report Share Posted June 7, 2017 Thanks Marcia. I have to test because this clay body "Standard 266" can bloat at cone 6 but ok at cone 5. Due to heavy iron content. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.