Kaolinwasher Posted May 4, 2017 Report Share Posted May 4, 2017 This is a porcelain made with 50% T-6 kaolin & 55% milled anoka sand and the Celadon glaze uses 56% anoka sand and together it makes a really good matching combo the glaze just glows with a soft blue green. I hope to start making some work with this combo now . Reduction fired to cone 8 Link to comment Share on other sites More sharing options...
terrim8 Posted May 5, 2017 Report Share Posted May 5, 2017 Looks so nice! Cone 8 is easier on the gas too. Link to comment Share on other sites More sharing options...