Kaolinwasher Posted November 18, 2016 Report Share Posted November 18, 2016 I am trying to make , sung celadons, and need bout 1% to 2% iron in the body. but i do not want to see specks i remember using red iron oxide and it left specks, I am leaning toward black iron oxide, < 1 micron or yellow ocher any advise would be nice Link to comment Share on other sites More sharing options...
glazenerd Posted November 18, 2016 Report Share Posted November 18, 2016 I am leaning toward black iron oxide correct Link to comment Share on other sites More sharing options...
Kaolinwasher Posted November 18, 2016 Author Report Share Posted November 18, 2016 thanks, I seen some that is < 1 micron Link to comment Share on other sites More sharing options...
glazenerd Posted November 18, 2016 Report Share Posted November 18, 2016 Wedging it in is going to be the issue. Link to comment Share on other sites More sharing options...
Kaolinwasher Posted November 19, 2016 Author Report Share Posted November 19, 2016 i will have to mix my own body, wet mix and screen at 100 mesh and dry on a bat, ya adding it to something would be a nightmare Link to comment Share on other sites More sharing options...