Mountain Meg Posted July 17, 2016 Report Share Posted July 17, 2016 Hi, We have been working months on,getting the pop off slip for 1 step naked raku just righ. I read that you could use a mason jar to mar the viscosity and then compare it when making other batches. If anyone has done this, please let me know. We just tried on a batch of our own, I would be really interested in any words of wisdom or advice. I thoroughly enjoy this process and seeing the results. Thank you, Mountain Meg Link to comment Share on other sites More sharing options...