Brijo Posted December 21, 2015 Report Share Posted December 21, 2015 I have load of mugs that were fired at cone 05 instead of cone 6 for the glaze firing. Half are glazed with amaco celadons and half amaco shinos. Is there any was save them? I am concerned about reglazing the shinos because there is no way to tell what the original color was. I cant tell for sure with all the celadons but some of them are obvious. Also, I don't want to waste the glaze (or my time) if there isn't a reasonable chance to salvage these pieces. Any help would be appreciated! Link to comment Share on other sites More sharing options...
bciskepottery Posted December 21, 2015 Report Share Posted December 21, 2015 Right now they are underfired; just refire the load to Cone 6. No need to reglaze. Link to comment Share on other sites More sharing options...
Brijo Posted December 21, 2015 Author Report Share Posted December 21, 2015 Thank you much for your prompt reply, you have really put my mind at ease! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.