A woman is selling this kiln for $750 I was wondering if that would be something worth buying or if that price a bit too high?
davidh4976
If you want to fire to cone 6, you may find that this kiln has trouble getting to cone 6, and you would be better getting a kiln rated for 8 or higher.
(See 1 other reply to this status update)