If I put some Iron oxide wash on a bisqued pot without glazing over it, would it stick after cone 6 firing, or might it come off and leave marks on your hands?
-
Hi RLC,
Welcome to the Forum!
You may create a new discussion thread under "Studio Operations and Making Work"
Select "Start New Topic" button, go.
I use red iron oxide to mark pots and test tiles so I can identify them later (which clay, which clear glaze, etc.); the pots have glaze over the marks, but not test tiles. The wash is stuck on after firing. Typically, some of the marking burns away...
Test and see if it works for you.
-