oldlady, I never handled this ashtray but the shop where I found it online in the description says it’s ceramic.
Have you ever used metallic acrylic paint? This paint can be baked, from the picture it looks good, I think I will make an experience with this.
https://ibb.co/Px2TGh2
Rae Reich, my problem is precisely the costs in using gold luster, I never used it before so I’m afraid I will have to try it out along with acrylic metallic paint.
Thanks for all your opinions. I’ve read that maybe with some types of acrylic paints applied affter glaze fire with a small sand in that area it’s possible to achieve a similar effect like in the picture. I think I will have to try.
I would like to know if anyone have an idea on how to use a glaze that looks like gold whithout using real gold luster.
Here is a picture.
https://ibb.co/SPpw1CF