Good morning all,
I am having consistent issues with Mayco SW colours; I love them but I can't seem to fire them right.
I have been using them on white stoneware (firing temp 1240ºC-1300ºC). I have applied one, two and three coats for testing and fired up to 1250 slowly and with a 30 min period at the end. I have an electric Kiln (rohde ecotop) that seems to work just perfectly.
I know I am doing somthing wrong but can't guess what; all my test tiles and pieces turn brown, I am not able to make the colours pop
The colors on the tiles are stoned denim and lavender, and the castle is tyger's eye
If anyone has any advice it would be very much appreciated, I am totally lost!
thank ou all for your time,