  1. Thanks everyone. Kelly your work is amazing. I thought of using it in the pit fire since the temperature can match luster firing, and I wasn't sure what will happen to pit fire effect if I will glaze the pots again ,and than apply luster (2 more firing cycles). I guess one has to try, that's part of potters life: trial and error.
  2. Hi, I did few pit fire testing, and I would like to add lusters (commercial ready) to the pots. Can that be done directly on the TS, before the firing? Or should I first do the pit fire, and than apply the luster and place in kiln firing it to the normal Luster temperature of ~600C? Thanks a million Iris
×
×