Hello, I was wondering if I have a kiln that goes up to cone 6 as the max then would it be fine if I use cone5-6 clay? I'm pretty new to all this so maybe it's a simple answer but I don't want to overwork my kiln ( i don't know if that's the correct term for it).
Thanks.
-
Hi Soup!
Perhaps you might move your question to Studio Operations and Making Work topic - might generate some discussion there.
Typically, new kiln will be able to reach its max rating, but at cost of more rapid wear on the elements; for cone 6 work, a kiln rated for cone 10 would be more suitable.
-