Can I low fire a 06 cone glaze and a bisque load in the same firing. That would be to use the 06 cone bisque schedule to glaze a few pieces?
-
i have done this kind of thing often. the important thing is that the firing is going to 06, therefore, anything that needs to go to 06 can be included. you should expect to go slowly so impurities can be fired out of the raw clay being bisqued.