  1. IN the middle of 100 glaze crystalline tests. No problem with shades of green, shades of blue. Looking for tips on two things. 

    #1 Oxidized red ground or crystals without the use of cadmium ( toxicity)

    #2 Yellows 

    #3 Creation of distinction of ground colors and crystal colors 

     

    1. glazenerd

      glazenerd

      Answered on your thread in Clay/Glaze zChemistry

    2. Mark C.

      Mark C.

      100 tests-now thats a bit of time

  2. IN the middle of 100 glaze crystalline tests. No problem with shades of green, shades of blue. Looking for tips on two things. #1 Oxidized red ground or crystals without the use of cadmium ( toxicity) #2 Yellows #3 Creation of distinction of ground colors and crystal colors Thanks all Perry Kenin
×
×