  1. I am always around with multiple timers on when firing, so I'm not so worried about lack of shutoff mechanism, but I see your point about the terminal. Maybe I'll fix it down the road! Thanks for your input.
  2. Hm.... Nope, no timer! Yeah, I did just use the power button last firing when the sitter stopped functioning, but the metal housing between the kiln jacket and the sitter box is super rusted, and I'm not sure that I should leave it there to keep disintegrating? Dunno!
  3. Hi you all, I have an ancient Paragon A82-B kiln with a Dawson kiln sitter that needs a new assembly tube. Usually I end up disregarding the kiln sitter anyways and just rely on the peephole cones, so is it possible that I could directly wire the switches so that I can fire without the kiln sitter? Is this a bad idea?
×
×