A couple thoughts
Did you have cones at same level as the thermocouple? Expect there to be warmer and cooler places...
Do you have an idea how fast the temp was rising the last hour or so? Note that the cones bend at lower temps when it's taking longer to get hotter - shoot for 2237F for cone 5.5 when the rate is 270F/hour
-
That's interesting because the temperature read 2237 at the hottest. It then started to move down. We have a call into the ConeArt company to see what we can alter or if we did something incorrectly. It must have gotten to close to 2295 or hotter because the cone 7 cone was bent all the way over as well. I don't know about the rate of temperature rise. Oh, so much to learn!
-