Hi Donna!
May I suggest you post your question to the "Studio Operations and Making Work" forum?
http://community.ceramicartsdaily.org/forum/22-studio-operations-and-making-work/
A couple thoughts
Did you have cones at same level as the thermocouple? Expect there to be warmer and cooler places...
Do you have an idea how fast the temp was rising the last hour or so? Note that the cones bend at lower temps when it's taking longer to get hotter - shoot for 2237F for cone 5.5 when the rate is 270F/hour
-
That's interesting because the temperature read 2237 at the hottest. It then started to move down. We have a call into the ConeArt company to see what we can alter or if we did something incorrectly. It must have gotten to close to 2295 or hotter because the cone 7 cone was bent all the way over as well. I don't know about the rate of temperature rise. Oh, so much to learn!
-
Each of the three columns is a different rate; to reach cone 5 where the rate is 27F/hour, stop at 2118F.
If the rate is much faster, e.g. 270F/hour, then take it up to 2205F
Your cone 7 will bend at 2194 if there's enough "heat work" (iow, slow rate).
I've fired one glaze load in my home kiln; I overfired on account o' my thermocouple reads a bit low, and my rate is slow as well...
-
The v6CF defaults to about 120 degrees per hour in the last 250 degrees of firing in cone fire mode. so their built in cone table will say 2232 I believe. I just replied with a post detailing some simple questions and we can send her the basic V6Cf technical setup. It’s pretty easy and since she is close likely will help correct the situation.
she will need to get familiar with fast glaze, slow glaze, etc..... as well
-
-
Hi All;
This weekend we did our first test firing for a new Cone Art Kiln. We used witness cones and fired to cone 6. We have a V6CF Bartlett Controller. When we opened the kiln my cone 5 witness cones were completely melted, the cone 6 and 7 cones were both completely layed over. The kiln controller had recorded a temperature of 2237 when it started to cool down. My cones are new as well. Any thoughts anyone? We are completely new to firing so want to figure this out before we do our first bisque firing.