  1. I have read that you can apply hair spray to the fired glaze to help the new glaze stick until it is fired . Is that a myth or does it work?
  2. I glazed a platter with Amaco Jade Celadon dipping glaze and fired it to ^6. It has a wide rim and I smugged the glaze, now I have a finger mark there. Can I re - glaze the rim with another glaze color, maybe something that will flow and then re - fire again to ^6. Also I would like to thank everyone for their prompt help with my other questions.