Jump to content

glazenerd

Members
  • Posts

    3,267
  • Joined

  • Last visited

10 Followers

Contact Methods

  • Website URL
    https://www.facebook.com/Clay-Tech-199305684284517/

Profile Information

  • Location
    St. Louis, Mo.
  • Interests
    Crystalline glaze chemistry. Porcelain, Stoneware, Fritware, 04 Colored Porcelain clay research & formulation.
    Ceramics Monthly Articles: Jan. 2018 Cation Exchange (plasticity), April 2018 SSA Clay Formulation, May 2018 Bloating and Coring.
    Feb. 2019 Ceramics Monthly- Clay Body Shopping Guide
    March 2019 Ceramics Monthly - Porcelain 201
    June 2019 Ceramics Monthly Clay Restoration
    Sept. 2019 Clay Memory
    Oct. 2019 Firing Programs

    Email: optix52@aol.com

Recent Profile Visitors

34,269 profile views

glazenerd's Achievements

Advanced Member

Advanced Member (3/3)

1.8k

Reputation

Single Status Update

See all updates by glazenerd

  1. Ordered technical grade/s of kaolins and one ball clay. Iron content is 0.08 which translates to super white porcelain.

    1. Show previous comments  3 more
    2. glazenerd

      glazenerd

      Mark- check your email.

    3. glazenerd

      glazenerd

      Iron content is a typo I just now seen: should read 0.18%

    4. Joseph Fireborn

      Joseph Fireborn

      How much $ per #? I am curious how cheap of stuff we are getting?

×
×