Posts
90 -
Joined
-
Last visited
Content Type
Profiles
Forums
Gallery
Everything posted by mdobay
-
From the album: 10/15/15
lidded jar -
Let me preface with I am fairly new and have only been throwing a few years and do not fire my own stuff. So its only a guess. The studio were I take classes, uses a gas kiln and I was thinking that color change and Crazing could have been caused by the reduction if the piece's was placed in a location of a draft?? My assumption is one of the reasons crazing happens is because a piece cools fast?
-
From the album: 10/15/15
-
From the album: 10/15/15
Cone 10, sight crazing I think from where it was placed in the kiln during the firing -
From the album: 10/15/15
First cone10 fire. love the gaze transitions -
From the album: 10/15/15
Lidded Jar with drift wood handle. -
-
-
-
From the album: 10/15/15
-
From the album: 10/15/15
lidded jars -
From the album: 10/15/15
Small jar