  1. Cutting a kiln shelf

    1. Dani

      Dani

      Has anyone sucessfully cut a kiln shelf? Have an 8 sided 'oval' and need an 8 sides 'circle'.

    2. MatthewV

      MatthewV

      Do you have a tile saw? With a wet diamond blade they aren't too hard to cut.

    3. Show next comments  3 more
×
×