Raku firing on a crisp Fall evening. A student project, one of my own, and some test tiles.
- Show previous comments 2 more
-
Luckily, yes I do.
-
did you like the results ?
-
Yes, fairly happy with the results. A vase, was supposed to have a blue lower portion, but turned out more copper-ish because of the reduction. I've accepted this part of Raku firing. The student project turned out great, but had some dunting, probably because of interior glaze thickness.