Status Updates posted by Nancy S.
-
C'mon, spring! I'm just itching to rewire the tin shop and get my own kiln up and running....
-
Hi! Quick question for you. I noticed on a post that you mentioned having worked with Standard 365 porcelain, and I'm wondering if you have any experience with 551? Also, how foolhardy would I be to go from stoneware to porcelain?
Thanks for your thoughts! (I can give you my email address if that's easier for you.)
-
I have not used 551. I have tried a couple of their other porcelain like bodies, though, and was not impressed. Their 365 throws beautifully, so I don't feel like theirs any reason to go to a white body that is supposedly more plastic. I do 45 pound planters with it with the 365 with no cracking or warping problems. The transition from stoneware to porcelain can be awkward, but you'll get used to it. Any particular reason you want to switch?
-