  1. 2016

    Various white earthenware pieces with transparent glaze fired to 1100oC.
    • Album created by Celia UK
    • Updated
    • 6 images
    • 5 image comments
    • 6 images
    • 5 image comments
  2. Celia's Efforts

    Some of my pieces made since retiring - 2012 to present.
    • Album created by Celia UK
    • Updated
    • 19 images
    • 11 image comments
    • 19 images
    • 11 image comments
  3. July 2019

    Haven’t been active on CAD for a long time - life just became very busy!
    Thought I’d create a new album of some recent work.
    • Album created by Celia UK
    • Updated
    • 6 images
    • 7 image comments
    • 6 images
    • 7 image comments
  4. Playing with mud 2016

    • Album created by Celia UK
    • Updated
    • 11 images
    • 6 image comments
    • 11 images
    • 6 image comments
  5. Winter 2016

    Latest kiln opening - White earthenware with texture slabs and copper oxide and cobalt carbonate wash under transparent glaze. Fired to 1080oC.
    • Album created by Celia UK
    • Updated
    • 6 images
    • 1 album comment
    • 5 image comments
    • 6 images
    • 1 album comment
    • 5 image comments
×
×