slip test
Using slip for texture and color disbursement. Spooned on and allowed to run off. After drying, a combination of a soft metal rib and sponge to rub off excess, and create textures. Slip had 0.25% cobalt carb added. Color is from nickel carb, magnesium carb, and Yellow Iron.