Cone 5 crystalline glaze.
 

Cone 5 crystalline glaze.



Single fire on custom porcelain clay recipe. Single fired, total ramp time 3.2 hours. Cone 5 peak temp. Notice the empty catcher. The recipe is simple, it is the clay producing the results.