9 29 16 green finally correct! 010
these pieces had come out too pale after their original firing. the green has finally been corrected and i now know that i have to put twice as much as i think on a piece and then add more. the central plate did not warp on its edges. i think it helps to center it and put other things nearby to avoid a hot or a cold spot that might cause warping. maybe???