ginko leaf tray done in Oribe green. recipe is not stable. proved with the vinegar test. tray sold to same person who bought the tree of life rectangular tray. new glaze on bottom tray. different recipe done with the new copper carbonate that is not like the old stuff. much weaker color. lots of re-fires with this glaze. have to get used to pouring it on thickly with my sprayer. have increased amount of copper to 5% since this piece.

From the album:

2016 fall pots

  • 12 images
  • 0 comments
  • 17 image comments

Photo Information for green spring show 008

Taken with EASTMAN KODAK COMPANY KODAK EASYSHARE C182 Digital Camera

  • 5.7 mm
  • 125000/1000000
  • f f/2.9
  • ISO 160
View all photo EXIF information

Recommended Comments

thank you, i have added more copper to make it  darker yet still transparent green.  the thickness and location of the veins in the leaves and are part of the reason i use them. the heart shape is the added attraction.  i believe that color is either 3 or 4% copper.  i now use 5.  see last photo this series.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.