Photo Information for carbon coring and other problems

Taken with Apple iPhone 5s

  • 4.2 mm
  • 1/30
  • f f/2.2
  • ISO 125
View all photo EXIF information

Recommended Comments

The iPhone 5 has its limitations, I broke about a third of the cups in half after testing the ring sound with a small metal hammer. The ones with a dull sound I broke in half and most show shiny black carbon deposits. also had very uneven firing, the way I loaded the kiln may have been some of the problem and my burners may need a little work.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.