Do all COE issues show themselves only in the glaze? Do all COE issues begin in the glaze?

Copyright

© TJA 2016
Sign in to follow this  
From the album:

USB Images

  • 25 images
  • 2 comments
  • 12 image comments

Photo Information for COE In clay


Recommended Comments

You should have went into XRF :D - go over to Saint Louis University & ask people in their Earth Sciences Dept. 

 As far as I know,  crack formation  - as you cool the melt, is rate dependent.  Here's two extremes with the same material:

Thick silica layers of Obsidian cool slowly  - not too many cracks. (deposited in volcanic layers)

Thin silica - Pele's Hair cools fast but it is thin (spewed out from the tail end of volcanic bombs!)

My 2 cents (prob. all its worth!)

 

 

Edited by terrim8

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.