Butterfly mug
This was a new take on a design I've been doing awhile. It may have spurred a new variation on several of my usual pots. I'm excited to see what comes of it.
The pattern at the bottom was created with paper resist and sgraffito. After bisque fired, black underglaze was applied and wiped back, then colorful accents added to the wings. It's finished with commercial ial glazes and fired to cone 6 in an electric kiln.