preeta 207 Posted July 4, 2016 Report Share marcia this is AMAZING!!! i love it. i always enjoy texture. Now off to your gallery to see if i can spot these in their full form. i have been checking your site out and am really getting interested in alternative firing. Quote Link to comment
SydneyGee 63 Posted November 8, 2016 Report Share Was this with sodium silicate? Mine totally failed on me, and I am devastated that it should be such a simple technique yet my form imploded on itself. Quote Link to comment
Marcia Selsor 2,017 Posted November 8, 2016 Report Share try my website http://www.marciaselsorstudio.com I have a video showing how its done. Quote Link to comment