Marko 191 Posted February 6, 2016 Report Share Very nice artwork Mea. I think I would like it more with the fish in color. What cone and how, if you would. I am a fan and I wish I could study under you. Quote Link to comment
GEP 2,653 Posted February 6, 2016 Report Share I brush white stoneware slip onto a dark stoneware bowl, then carve through the white slip. Glazed and fired to cone 6/electric. Thanks for the nice comments, Marko! Quote Link to comment