Michael's Bailey's Orange red Base Glaze from his book ^6 Glazes

Potash Feldspar 46.7

Kaolin 4

Bentonite 2

Bone Ash 15

Lithium Carb. 4

Talc 16.9

Silica 11.4

total 100.0

 

Red Iron Oxide 11.5%

hold at ^6 for 20 minutes and soak again at 1900 for 30 minutes

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.