Wheel thrown white stoneware platter, underglazes with black underglaze outline, dotted accents. Clear glaze. 12" diameter.

From the album:

New ^6 Work 2015 (2)

  • 6 images
  • 0 comments
  • 13 image comments

Photo Information for 039 Sunburst Garden Platter

Taken with Canon Canon PowerShot A1100 IS

  • 6.2 mm
  • 1/30
  • f f/2.7
  • ISO 320
View all photo EXIF information
 Share


Recommended Comments

Thanks, Marko.  These are all bisqued at ^07 with underglazes on and glaze fired to ^6 oxidation. Yes all the designs are freehand, although I block it out into 8ths to get started. The colored underglaze,  the blackline underglaze and the dotted accents take me about 90 minutes to apply. The platter is 12" diamete.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.