Pink to purple bowl
The glaze is the standard silky white crystalline glaze I've been using a lot lately. The center of the bowl was sprayed with a pale green crystalline glaze to define the texture of the fluted pattern carved lightly into the porcelain. For unknown reasons, this sprayed on glaze fumed the white rim of the bowl to an almost fluorescent pink, and crystallized pink flowed down and collected in the center of the bowl