The glaze is the standard silky white crystalline glaze I've been using a lot lately. The center of the bowl was sprayed with a pale green crystalline glaze to define the texture of the fluted pattern carved lightly into the porcelain. For unknown reasons, this sprayed on glaze fumed the white rim of the bowl to an almost fluorescent pink, and crystallized pink flowed down and collected in the center of the bowl -
From the album: newer work
A sake set of white-glazed porcelain. A light spray of iron glaze helps to define the flutes carved into the forms. -
From the album: newer work
These porcelain yunomis are fluted and glazed with a pale green ash glaze on the exterior, and a clear glaze on the interior, overlaid with ash glaze a distance down from the rim.