Tripod Pot
This little bisque tripod pot was formed using Sandi Pierantozzi's method. Slab rolled, gutter cover rolled into the slab with a pony roller then formed into a cylinder and pinch the feet. I added the lid using the same method except it was four "feet" and using a different gutter cover for the texture.