DSCF3704
porcelain/stoneware i have been working on a clay formula or 3 for about 4 years and trying to get some input on how many potters actually like the clay there are using. to this point i have made a white porcelain/stoneware clay that dose not warp while drying,[ with utilitarian wares ] no need to wire off plastic bats . [ released its self ] air drying. [ no need to cover it up ] and so far doesn't have any cracking issues. [ example ], i threw 25 4.5 lbs 12 inch plates on plastic bats, air dried them , did not wire them of the next day some had already released themselves and were as flat as the bat. trimmed them all. bisqued them and fired to cone 10. i would appreciate any comments . thanks tobias