commercial dinner plate clear glaze W bubble
bubbles on the bottom of a commercial dinner plate whiteware. bubbles are smaller and somewhat more dispersed, but still visible as small spheres. 200x magnified.
bubbles on the bottom of a commercial dinner plate whiteware. bubbles are smaller and somewhat more dispersed, but still visible as small spheres. 200x magnified.