purple bowl dark spot W bubbles
spherical bubbles in a transparent glaze fired cone 10 oxidation. dark blemish on otherwise white porcelain gives some additional contrast to show bubbles. 200x magnification.
spherical bubbles in a transparent glaze fired cone 10 oxidation. dark blemish on otherwise white porcelain gives some additional contrast to show bubbles. 200x magnification.