I do a lot of this nautical wave pattern on my pieces. this was the first cup I stacked 2 of the patterns on top of each other. I actually meant to glaze the interior with a different liner but I really liked the combination anyway after it was fired. applied engobe, with sgraffito, commercial glazes. Fired ^6 electric.