Made loosely following a Simon Leach video tutorial

Runyan Wheatstone clay

Waterfall brown dunk, angle dipped in Ron Roy's Clear

Grinding surfaces were left unglazed, and a triangular shelf stilt was used to hold the pestle upright on its unglazed end for glaze firing

Copyright

© 2014 Stell Michelsen
From the album:

Session 2

  • 9 images
  • 0 comments
  • 1 image comment

Photo Information for Mortar and Pestle

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.