Made as a gift for a local café - Julienne Tomatoes

Standard 300 Brown clay

Lined with Nutmeg, bottom dip of Turquoise Matte, top dip of Stone White, no overlap

Tomato: Amaco velvet underglaze, 2 coats radiant red and leaf green, waxed over for glaze dipping

Copyright

© 2014 Stell Michelsen
From the album:

Session 2

  • 9 images
  • 0 comments
  • 1 image comment

Photo Information for image

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.