2010. This piece is a white stoneware sculpture, finished with artists oils. I had made this about 10 years previously, but it exploded in my kiln (not dry), and so did my desire to continue sculpting. It was 10 years before I decided to try again.

Sign in to follow this  
From the album:

Sculpture

  • 6 images
  • 0 comments
  • 1 image comment

Photo Information for Christie

Camera information

View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.