Translucent Plate



Test Plate using experimental porcelain

From the album:

some work

  • 8 images
  • 0 comments
  • 18 image comments


Recommended Comments

Very translucent. It's hard to photograph that. If you're familiar with them, how does it compare to Frost and Southern Ice, the two most translucent porcelains I've ever seen?

 

Jim

Link to comment

Offcenter,

I agree, it is difficult to show. I thought your video worked well, movement seems to help.

I have not yet used Frost or Ice, but I have done many tests using the same New Zealand kaolin, and as far as I can tell using this clay body with NZ kaolin should be more translucent than them, but only because this clay is so highly fluxed and has lower clay content. It has to be fired in a form, or on something flat, and is actually glassy when mature.

Thanks for your question.

And thanks Trina

 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.